Swipe or use the arrows to view product images.
38mic Laser Thermal Lamination Film-Bt5 (FSEKO-3D true color holographic)
| Price | $2300.00 |
|---|---|
| Min Order | 1 Ton |
| Availability | In Stock |
| Shipping From | Guangdong, China |
| Popularity | 359 people viewed |
Model NO.:
EKO38MIC
Type:
Holographic Film
Material:
BOPP
Processing Type:
BOPP+EVA
Hardness:
Soft
Transparency:
Transparent
Thickness:
30-40mic
Trademark:
FSEKO
Transport Package:
Carton Box(+Pallet If Needed)
Specification:
SGS RoHS
Origin:
Foshan, China
HS Code:
3920
Product Description
*Material
Surface layer: BOPP
Glue layer: EVA adhesive
*Specification
Thickness: 30mic/40mic
Width: 300~1800mm
Length: 200~3000m
Paper core: 25.4mm (1 inch), 58mm(2.25inches), 76mm(3 inches)
Bonding: Less than 2
*Process parameter:
Equipment for thermal film: Dry and wet film laminator
Lamination temperature: 95~105c
Roller pressure: 10-20mpa
Speed: 8-20 m/min
*Directions for using BOPP thermal laminating film:
Normal process temperature is 90c-105c, roller pressure and temperature vary with different types of paper, ink and machines.
When using the film for the first time or do other treatment, try a small volume before mass laminating.
Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder.
Make sure put the material in a low-temperature, dry place.
*Packaging:
Surface layer: BOPP
Glue layer: EVA adhesive
*Specification
Thickness: 30mic/40mic
Width: 300~1800mm
Length: 200~3000m
Paper core: 25.4mm (1 inch), 58mm(2.25inches), 76mm(3 inches)
Bonding: Less than 2
*Process parameter:
Equipment for thermal film: Dry and wet film laminator
Lamination temperature: 95~105c
Roller pressure: 10-20mpa
Speed: 8-20 m/min
*Directions for using BOPP thermal laminating film:
Normal process temperature is 90c-105c, roller pressure and temperature vary with different types of paper, ink and machines.
When using the film for the first time or do other treatment, try a small volume before mass laminating.
Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder.
Make sure put the material in a low-temperature, dry place.
*Packaging:
- Similar Products
$0.23
2000 Square Meters (MOQ)
Transparent Metalized Zns Holographic Pet Polyester Hologram Film 16um
Zhejiang Zhongjie Packaging Material Co., Ltd.
$0.27
5000 Square Meters (MOQ)
UV Offset 3D Holographic Film 3D Hologram Foil Multiple Lens Film
Wenzhou Zhanxin New Materials Technology Co., Ltd.
Negotiable
100 Pieces (MOQ)
New Ovi Overlay Hologram UV State Hologram
Shenzhen Sijie Technology Co., Ltd.
Negotiable
20 Pieces (MOQ)
Connecticut Teslin Paper Sheet CT Micro Holes Sheet Paper
Shenzhen Sijie Technology Co., Ltd.