Negotiable
1 unit (MOQ)
Galvanized Steel Wire Making Equipment Supplier
Wuxi Xinrun Industrial Furnace Co., Ltd.
Swipe or use the arrows to view product images.
Automatic Closed Pretreatment Wire Rod Pickling Phosphating Line
| Price | $800000.00 |
|---|---|
| Min Order | 1 Set |
| Availability | In Stock |
| Shipping From | Tianjin, China |
| Popularity | 319 people viewed |
Model NO.:
Beest O-25
Warranty:
18 Month
Type:
Coating Production Line
Coating:
Coil Coating
Substrate:
Steel
Certification:
CE, ISO
Condition:
New
Material:
Pph
Dia. of Wire:
2.0--40mm
Key Selling Point:
Easy to Operate
Wire Rod Weight Per Hook:
5t
Height:
13m
Selling Units:
Single Item
Trademark:
Beest
Transport Package:
Container
Specification:
70000t/y--400000t/y
Origin:
China
HS Code:
8479899990
Product Description
AUTOMATIC WIRE ROD PICKLING AND PHOSPHATING LINE
Equipment Specifications
| Item | Index | Mark |
| annual output | 100,000 tons | 7200 hour |
| Hook type | 1 set/hook | Each manipulator 1 wire rod |
| Equipment height | About 9.5m | |
| Equipment width | About 22m | |
| Equipment length | About 57m | |
| hanger rail circumference | About 126m | |
| Turning radius | 4m | |
| No. of Manipulator | 10 sets | 9 Use 1 spare |
| Speed of Manipulator | 20m/min | |
| No. of tank | 19 sets | |
| Tunnel structure | Fully enclosed structure | |
| Number of loading carts | 2 sets | 1 for loading and 1 for unloading |
| Tank service life | >10 years | |
| Steel structure installation method | High-strength bolt connection | |
| Acid mist treatment method | Double tower series spray |
4.2.01:Loading
Purpose:Send the steel wire rod to the production line;
Time:About 3 minutes.
4.2.02:Water seal & Degreasing
Purpose: Degreasing and cleaning the wire rods entering the production line to wash away the oily attachments on the surface;
Medium:Degreasing liquid;
Temp.:about 60-80ºC(KMnO4 90-95ºC)
Time:About 3 minutes.
4.2.03:Rinsing-1
Purpose: Clean the wire rod after degreasing to remove some oils etc.
Medium: water from Rinsing-2
Temperature: Hot water
4.2.04:Pickling-1~4
Purpose:Remove the oxide layer on the surface of the wire rod, chemical reaction;Medium:HCl
Temperature:about 35ºC-60ºC(According to different pickling process)
Time:Total about 30 minutes.
4.2.05:Rinsing-2
Purpose: Clean the wire rod after pickling to remove some residual acid and ferrous iron;
Medium: water from Rinsing-3
Temperature: Hot
Time: 0.5~1 minutes.
4.2.06:Rinsing-3&4
Purpose: Further cleaning the wire rod surface;
Medium: water from High pressure spraying-1;
Temperature: normal
Time: 0.5~1 minutes.
4.2.06:High pressure spraying-1
Purpose: To perform high-pressure washing on the inner and outer surfaces of the wire rod to remove residual acid and ferrous ions on the surface of the wire rod;
Medium: industrial water;
Temperature: normal
Time: 0.5~1 minutes.
4.2.07:Surface conditioning
Purpose: to remove most of the ferrous iron and iron compounds remaining on the surface of the wire rod after pickling;
Facilitate the formation of phosphating film with fine and compact grains;
Improve the adhesion of phosphate coating;
Medium: oxalic acid
Temperature: 30~60ºC
Time: 2~3 minutes.
4.2.08:phosphating 1~2
Purpose: to form a phosphate film on the surface of the wire rod;
Medium: zinc phosphating solution
Temperature: 75-90ºC
Time: about 8 minutes (low carbon);
about 5 minutes (high carbon)
4.2.09:High pressure spraying-2
Purpose: To remove the phosphating liquid and slag on the wire rod after phosphating;
Medium: overflow water from Rinsing-5
Temperature: normal
Time: 0.5~1 minutes.
4.2.10:Rinsing-5
Purpose: To remove the phosphating liquid and slag on the surface of the wire rod after spraying-2;
Medium: tap water
Temperature: normal
Time: 0.5~1 minutes.
4.2.11:Boronizing
Purpose: Neutralize the residual acid on the surface of the wire rod. Formed a loose and porous puffed coating on wire rod surface convenient for wire drawing.
Medium: Borax
Temperature: ≤95ºC
Time: 0.5~1 minutes.
4.2.12:Liming
Purpose: Neutralize the residual acid on the surface of the wire rod. Formed a liming coating on wire rod surface convenient for wire drawing.
Medium: tap water
Temperature: 85-95ºC
Time: 2-3 min minutes.
4.2.13: Saponification
Purpose: To saponify the surface of the wire rod;
Medium: soap
Temperature: ≤80ºC
Time: 1-2min minutes.
4.2.14:Drying
Purpose: Dry the surface of the wire rod;
Medium: Natural gas
Temperature: ≤170ºC(can up to 200ºC)
Time: about 3-5 minutes.
4.2.15:unloading
Purpose: to perform offline operations on processed wire rods;
Time: about 3-5 minutes.
- Similar Products
Negotiable
1 unit (MOQ)
Galvanized Steel Wire Make Equipment Manufacturer
Wuxi Xinrun Industrial Furnace Co., Ltd.
$8000.00
1 Piece (MOQ)
Continuous Aluzinc Line/ Galvanized Equipment/Galvanizing
Maker Metallurgy Technology Co., Ltd