Menu
Global B2B sourcing platform
Verified suppliers and manufacturers

Surfactant Lycra Protector Post Finishing Auxiliary for Elastic Denim

Price $1.70
Min Order 500 kg
Availability In Stock
Shipping From Shandong, China
Popularity 328 people viewed
Model NO.:
GR-L101
CAS No.:
64422-66-8
Certification:
REACH
Environmental Protection:
Yes
Color:
White
Kind:
Protective Agent
Appearance:
Powder
Application:
Pretreatment Auxiliary, Dying Auxiliary, Post-Processing Auxiliary
Name:
Lycra Protective Agent
Active:
100%
Samples:
Available
MOQ:
500kgs
Trademark:
green
Transport Package:
25kg Bag
Specification:
Protective Agent
Origin:
China
HS Code:
5007201900
Product Description
Lycra Protector GR-L101

Recommend technology in denim washing process

1. Desizing process:
Add GR-L101 0.5g/L (500g/machine), soap oil HP6, 0.2-0.5g/L, warmed to 50-60ºC, run 8-10 minutes, then drain cleaning.

2. Enzyme Washing process:
GR-L101, 0.2g/L (200g/machine), warmed to required temperature 40-50 ºC (or without warm), add acid or neutral cellulase (powder or liquid), adjust pH value in advanced if use acid cellulase. Washing time be based on sample plate requirement, drain cleaning after right edition.

3. Sodium hypochlorite bleaching process:
Caustic soda, 0.5-1g/L ( 500-1000g/machine, only add when heavy bleaching); spandex protector GR-L101, 1-1.5g/L (1000-1500g/machine) before adding bleaching liquor, add GR-L101, run for 3-5 minutes, warm up while running, add bleaching liquor to 50ºC in batches, add 1/5 bleaching liquor for the first time, run for a few minutes, add the remaining 4/5 bleaching liquor for the second time, according to the specific process time drift, drain liquor while flooding water after bleaching be finished, washed for 3 minutes, add dechlorination deodorant 0.3-0.5g/l, 25 ºC ×5-10min dechlorination treatment, water washing, dehydration and drying.
 
Application

Application on garment dyeing

1. H2O2 bleaching technology:
     
Caustic Soda2-3g/L
H2O2 (35%)7-15g/L
GR-L1011-2g/L
Temperature-Time80-85ºC×60-120 min
Bath ratio1:10-20