High shrinkage yarn
PROPERTIES
Modifed polyester filament, the shrinkage rate can reach 30% to 70%. It can be compounded with other yarns with different shrinkage rates, thus the fabrics made from those could have better hand touch after finishing. It can also be mixed with other synthetic fibers or natural fibers of different shrinkage rate to make the fabric a concave-convex feeling.
APPLICATION
Apparel, home textiles, automotive interiors, etc
MAIN SPECIFICATION
30D/12F,60D/24F,90D/36F
More informations ,please contact with us .