Name | Soft magnetic alloy wire | ||
Grade | Soft magnetic alloy | 1J06,1J12,1J17,1J18 ,1J30,1J76 ,1J51,1J54,1J46,1J80,1J87 | |
Permalloy | 1J50, 1J79 ,1J85, 1J77 | ||
Fe-cobalt alloy | 1J22 ,1J36 ,1J38 ,1J55 | ||
Size | Sheet | 3.5-40/mm | |
Strip | 0.2-3.5/mm | ||
Pipe | 8.0-180/mm | ||
Bar | 8.0-180/mm | ||
Wire | Custom | ||
Density | 8.2 g/cm3 | ||
Thermal Expansion Coefficient (20~100ºC) | 8.2*10-6 /ºC | ||
Curie Point | 498ºC | ||
Volume Resistivity (20ºC) | 45μΩ.cm | ||
Thermal Conductivity | 16.5W/m. ºC | ||
InitialMagnetic Permeability | Min.8.0mH/m | ||
MaximumMagneticPermeability | Min.50mH/m | ||
CoerciveForce | Max.10A/m | ||
SaturationMagneticFluxDensity | 1.5T |
Chemical Composition | ||||||||
C | P | S | Cu | Mn | Si | Mo | Ni | Fe |
≤0.03 | ≤0.020 | ≤0.020 | ≤0.020 | 0.30-0.60 | 0.15-0.30 | 4.8-5.2 | 79.0-81.0 | margin |
MEAN COEFFICIENT OF LINEAR EXPANSION | ||||||||
20-100ºC | 20-200ºC | 20-300ºC | 20-400ºC | 20-500ºC | 20-600ºC | 20-700ºC | 20-800ºC | 20-900ºC |
12.8-13.0 | 12.5-12.7 | 13.1-13.4 | 13.4-13.8 | 13.9-14.4 | 14.2-14.8 | 14.5-15.2 | 15.0-15.6 | 15.5-15.6 |








A3: We have our own production and inspection equipment. There are always pre-production samples before mass production, and there are always final inspections before shipment.Quality is the tenet of our company.
Q4. Do you provide samples?
A4: Yes, we provide samples if needed, but customers need to pay the sample fee.
Q5. Can I visit your factory before ordering?
A5: Of course, you are welcome to visit the factory.