Swipe or use the arrows to view product images.
Melamine Moulding Compound MMC Made From China Factory
| Price | $1450.00 |
|---|---|
| Min Order | 20 Tons |
| Availability | In Stock |
| Shipping From | Henan, China |
| Popularity | 310 people viewed |
Model NO.:
A5
CAS No.:
108-78-1
Formula:
C3h6n6
EINECS:
203-615-4
Color:
White
Name:
Melamine-Formaldehyde Resin
Other Name:
Mf, Melamine Moulding Compound
Type:
White, Black, Red, Blue, Pink or OEM Color
Applicatio:
Tableware or Dinnerware
Trademark:
premtec
Transport Package:
25kgs Bag
Origin:
China
HS Code:
2933610000
Product Description
Melamine Moulding Compound MMC Made From China Factory
A polymer produced by the reaction of melamine with formaldehyde.Also known as melamine formaldehyde resin, melamine resin.The English abbreviation MF.The cross-linking reaction occurs during processing and molding, and the product is a non-melting thermosetting resin.It is often commonly referred to as amino resin with urea-formaldehyde resin.
| CAS No.: | 108-78-1 |
|---|---|
| Formula: | C3h6n6 |
| EINECS: | 203-615-4 |
| Type: | Synthesis Material Intermediates |
| Appearance: | Powder |
| Quality: | Industrial |
Specification
Item | Index | Test Result |
Appearance | White Powder | Qualified |
Mesh | 70-90 | Qualified |
Moisture% | <3% | Qualified |
Volatile Matter% | 4.0 | 2.0-3.0 |
Water Absorption(cold water),(hot water) Mg,≤ | 50 | 41 |
65 | 42 | |
Mold Shrinkage% | 0.5-1.0 | 0.61 |
Heat Distortion TemperatureºC | 155 | 164 |
Mobility(Lasigo) mm | 140-200 | 196 |
Charpy Impact Strength KJ/m2 ≥ | 1.9 | Qualified |
Bending Strength Mpa ≥ | 80 | Qualified |
Uses
1)melamine-formaldehyde resin
2)docorating plates
3)amino plastic
4)corehent agent
5)intensifier of paper currency
6)texitile assistant
7)water-saving agent of cement
8)leather tanning agent
Packing: 25kg/bag or JUMBO bag
Delivery Time: 3-10 days after receiving TT payment
Delivery Time: 3-10 days after receiving TT payment
Storage: Store in a cool, ventilated warehouse. Keep away from fire and heat sources. It should be stored separately from oxidants and acids, and avoid mixed storage. The storage area should be equipped with suitable materials to contain the leakage.
- Similar Products