Menu
Global B2B sourcing platform
Verified suppliers and manufacturers

Polyurethane Foam for Integral Skin PU Foam System

Price $2.25
Min Order 200 kg
Availability In Stock
Shipping From Shandong, China
Popularity 400 people viewed
Model NO.:
ZHD-8008C
CAS No.:
9009-54-5
Formula:
C3h8n2o
EINECS:
9003-11-6
Source:
Organic Acids
Appearance:
Viscous Liquid
Grade Standard:
Industrial Grade
Colour:
White
Usage:
Automobile Seat, Backrest and Headrest
Features:
High Elasticity
Color:
White
Viscosity at 25°c, Cps:
4500±500
Specific Gravity@25ºC:
1.05±0.05
Free Rise Density,Kg/M3:
30-60
Water Content:
1.5-2.0
Cream Time (S):
38-43
Gel Times (S):
75-80
Mold Temperature (ºC):
50-55
Demould Time (Min):
6-7
Frd (Kg/M3):
150-170
Mold Foam Density (Kg/M3):
350-400
Core Density (Kg/M3):
200-250
Urface Hardness Shore a:
70±5
Trademark:
Huide
Transport Package:
Steel Drum/IBC/Tank
Specification:
200kgs
Origin:
Zibo, China
HS Code:
3907299090
Product Description
 Polyurethane Foam for Integral Skin PU Foam System
 
Integral skin foam system
Application field: Automobile and Furniture, used as Armrest, Children's seat, Fitness equipment, etc.

Features: 1. Independent closed bubble combination, low density and small thermal conductivity of rubber material, so it has excellent thermal insulation performance.
2. The surface is skinned, so the water vapor can not pass through, and there is no need to add a steam barrier, the outer wall will not condense, and the water absorption is low.
3. Soft feel, good elasticity, high strength, smooth surface, easy, economical, fast, elegant, neat and clean installation
4. Flame retardant, self extinguishing and non delayed combustion, meeting fire protection requirements.
5. It is applicable to a wide range of temperatures and has excellent low temperature resistance,
6. It has no CI or chemical fiber and will not cause skin allergy.
7. It has the strong quality of stretching and bending, can withstand tearing and rough force transmission, and will not be damaged under severe conditions.
8. Good shock absorption and sound absorption



SPECIFICATION
ItemZHD-8008C/CAR
Ratio(A/B)100/40-45
Cream time (s)38-43
Gel times (s)75-80
Mold temperature (ºC)50-55
Demould time (min)6-7
FRD (kg/m3)150-170
Mold foam density (kg/m3)350-400
Core density (kg/m3)200-250
Surface hardness Shore A70±5