Swipe or use the arrows to view product images.
High Strength Concrete Used Hook End Steel Fibres
| Price | $1100.00 |
|---|---|
| Min Order | 1 Ton |
| Availability | In Stock |
| Shipping From | Shanghai, China |
| Popularity | 253 people viewed |
Model NO.:
SAP 6560 GHW
Material:
Metal
Type:
Steel Fibre
Tensile Strength:
1150MPa
Types:
Loose/Glued
Function:
Strengthen, Fireproof
Certification:
ISO
Trademark:
SAPEN
Transport Package:
Bag+Pallet
Specification:
D: 0.55-0.9mm, L: 30-60mm
Origin:
Shanghai, China
HS Code:
7326901000
Product Description
Hooked End Steel Fibre
(Loose / Glued)
Description (Loose / Glued)
Hooked end steel fibre is made of cold-drawn wire. In the concrete mixture, add right amount steel fibres can be mixed into a kind of special jetting as well as casting concrete, namely steel fibre reinforced concrete. Compared with general concrete, steel fibre concrete has a great improvement in tensile strength, flexural strength, abrasion resistance, impact resistance, fatigue resistance, toughness, crack resistance and antiknock performance.
Application
- Mortar reinforcement
- Ground, bridge, highway pavements dam
- Railway sleeper
- Shotcrete, tunnel and mine
- Improve structural strength
- Reduce steel reinforcement requirements
- Reduce crack widths and control the crack widths tightly, thus improving durability
- Improve impact- and abrasion-resistance
- Improve freeze-thaw resistance
| Product-code | L(mm) | D(mm) | Tensile strength(MPa) | Aspect ratio |
| SAP 6560 GHW | 60 | 0.9 | ≥1150 | 67 |
| SAP 8060 GHW | 60 | 0.75 | ≥1150 | 80 |
| SAP 6535 GHW | 35 | 0.55 | ≥1150 | 64 |
| Other | customizable | customizable | customizable | customizable |
Guideline for use
- Dosage: depend on the application and minimum dosage range is 20kg/m3-70kg/m3.
- Mixing: put sand and stones into the hopper. While turning the sand and stones into the hopper, mix the proper amount of loose steel fiber, and then add the cement.Hang the sand, stones, steel fibers, and cement from the hopper into the mixing table and dry mix for 2 minutes, then add water to mix for 2 minutes. Glued steel fiber should be added after water mixed to dissolving glue.
- Put the evenly mixed fiber concrete into the carriage and transport it.
- The concrete pouring and laying should be tamped and compacted.
25kg/Bag, 1200kg/Pallet, 24 T/ 20' Container. Other packing way according to customer's requirements.
Shotcrete with easy-mix Steel Fibre
- Similar Products
$0.32
5000 Square Meters (MOQ)
Needle-Punched Geotextiles 100% Polypropylene Staple Fibers
Feicheng Lianyi Engineering Plastics Co., Ltd.
$10.00
100 Square Meters (MOQ)
Lightweight and Flexible Carbon Fiber Mesh for Easy Construction Installation
Jiangsu Nongchaoer Composite Material Co., Ltd.