Shot peening is a method of cold working a part surface under a spray or blast of round shot to increase a part's fatigue life. Fatigue failures usually begin on the surface of a part. Shot peening makes tiny dents or curves on the surface of the metal. This creates a layer of compressive stress, which delays the creation and growth of fatigue cracks. In some instances, peening can increase the fatigue life of a part by 2,000% or more.


Chemical composition:
| Item | Main elements (%) (min) | Impurities (≤)%(max) | |||||||
| Zn | Al | Mg | Ni | Fe | Pb | Cd | Cu | TTL | |
| ZA2Mg | REMAINING | 1.0-3.0 | 0.001-0.005 | - | 0.08 | 0.01 | 0.002 | 0.05 | 0.1 |
| ZA3Mg | REMAINING | 2.0-4.0 | 0.001-0.005 | - | |||||
| MLZ-1 | REMAINING | 0.005-0.5 | 0.005-0.02 | - | |||||
| MLZ-2 | REMAINING | - | - | 0.001-0.004 | |||||
Product Features:
| Item | Hardness HV0.1 |
| ZA2Mg | ≥ 35 |
| ZA3Mg | ≥ 42 |
| MLZ-1 | ≥ 70 |
| MLZ-2 | ≥ 25 |
Diameter: 0.3mm≤Ф≤1.60mm
| DIAMETER | PERMISSIBLE |
| (MM) | VARIATION |
| 0.3≤Ф<0.6 | +0.00,-0.02 |
| 0.5≤Ф≤1.00 | +0.00,-0.03 |
| 1.00≤Ф≤1.6 | +0.00,-0.04 |
| 1.60<Ф≤2.00 | +0.00,-0.05 |
| 2.00<Ф≤2.50 | +0.00,-0.06 |
Product packing:
| Hard paper drum | 20-400 kg |
| Plastic spool | 10-25 kg |
| bundle | 5-40 kg |


Our wire is an ideal material to make shot peening materials.
Zinc alloy has a wide range of applications with high-precision surface treatment and is safer and more environmentally friendly in use.
We are looking forward to your cooperation!