Tin base Babbitts are considered superior to Lead base alloys for most applications because they are easier to pour and provide a good bond between the bearing shell and lining. In this process, Babbitt ingots are melted and then poured into bearing cavities, allowed to harden, and then the surface is machined down to meet required tolerances.


Product code: solder wire
Chemical composition:
| ITEM | Melting Range (ºC) | Elements (%) | |||||||||||
| Sn | Ag | Cu | Sb | Pb | Cd | Fe | As | Al | Zn | Bi | TTL Impurities | ||
| S-SnCu0.7 | 227 | REMAINING | 0.1 | 0.5-0.9 | 0.1 | 0.05 | 0.0012 | 0.02 | 0.03 | 0.001 | 0.001 | 0.015 | 0.2 |
| S-SnCu0.3 | 227~235 | REMAINING | 0.1 | 0.2-0.4 | |||||||||
| S-SnCu3 | 227~310 | REMAINING | 0.1 | 2.5-3.5 | |||||||||
| S-SnAg1Cu0.5 | 217~227 | REMAINING | 0.8-1.2 | 0.3-0.7 | |||||||||
| S-SnAg3Cu0.5 | 217~220 | REMAINING | 2.8-3.2 | 0.3-0.7 | |||||||||
| S-SnAg4Cu0.5 | 217~219 | REMAINING | 3.8-4.2 | 0.3-0.7 | |||||||||
| S-SnCu0.7Ag0.3 | 217~227 | REMAINING | 0.2-0.4 | 0.5-0.9 | |||||||||
| S-SnCu4Ag1 | 217~353 | REMAINING | 0.8-1.2 | 3.5-4.5 | |||||||||
| S-SnCu6Ag2 | 217~380 | REMAINING | 1.8-2.2 | 5.5-6.5 | |||||||||
| S-SnSb5 | 235~240 | REMAINING | 0.1 | 0.05 | |||||||||
Size: 295*20*13mm
Product packing:
20kg per carton.


Widely used in a variety of wave soldering and manual welding of television, audio, capacitors, circuit boards, and communications equipment. and look forward to your cooperation!